Makina otentha opangira nkhungu amatchedwanso makina opangira nkhungu otentha. The basi kulamulira kwa kufa-akuponya otentha nkhungu makina nkhungu kutentha ndi njira singasiyanitsidwe mu zamakono zamakono kufa kuponyera. Ndi ntchito ziti za kufa-akuponya otentha makina nkhungu mu ulamuliro kutentha kwa nkhungu kufa-akuponya?
Mu Preheating Gawo la Die kuponyera Nkhungu, Udindo Wa Hot Nkhungu Machine
- Kutentha nkhungu kumatha kuchepetsa kuchuluka kwa nkhungu zotentha, kukonza magwiridwe antchito komanso kuchepetsa zinyalala;
- Kutentha nkhungu kumatha kuchepetsa kutentha kwa chitsulo chosungunuka pachikombole chofera, kutalikitsa nthawi yamatenthedwe otopa mu nkhungu, ndikuwonjezera moyo wa nkhungu;
- Kukonzekera kupanga nkhungu akhoza kupanga kusiyana kwa gawo lotsetsereka la nkhungu kukulitsa ndikusintha, ndikuletsa chitsulo chosungunuka kuti chisabowole gawo lotsetsereka ndikuthamangitsa nkhungu;
Makina otentha otentha otentha otentha akamaumba nkhungu amatha kuchepetsa kutentha kwa mafuta ndikuchepetsa kutentha kwa chitsulo chosungunuka. Nthawi zambiri ntchito mu yokoka zitsulo kuponyera nkhungu. Pulogalamu ya kufa kuponyera Makina otentha amatha kutentha nkhungu mofananamo ndipo ali ndi ntchito yoziziritsa nkhungu kuti zitsimikizire kuti kutentha kwa nkhungu ndikuchepetsa kutentha kwa chitsulo chosungunuka; Ndi zida muyezo kupanga aloyi zotayidwa woonda-mipanda ndi amatha kuumba aloyi mankhwala enaake a.
Ntchito Ya The Die Die Casting Hot Mold Machine Panyengo Yotentha Yoyendetsa Imfa
Ngati kutentha kwa nkhungu kumakhala kotsika kwambiri kapena kotsika kwambiri, kumapangitsa zolephera monga kukula kosakhazikika kwa kuponyera, kuchuluka kwakukana kwambiri ndikuchepetsa kutulutsa. Mukamatsanulira mipanda yolimba, kutentha komwe kumatumizidwa mu nkhungu nthawi zambiri kumakhala kochepa kuposa kutentha kotayika ndi nkhungu, kotero kuti kutentha koyenera sikungafikiridwe, ndipo makina opangira nkhungu otentha amafunika kuwonjezera kutentha kuti asunge nkhungu kutentha zonse.
Momwe kutentha kwa nkhungu kumakhudzira kutaya kwa kufa kuli ndi zinthu zotsatirazi.
Kutentha kwambiri nkhungu kumatha kuyambitsa:
- (1) The kuthamanga pakati ndi waukulu kwambiri, ndipo kuponyera ndi kovuta kuti demould;
- (2) Ntchito yowonongeka ya wotulutsa nkhungu (yotchedwa nkhungu yotulutsa zinthu) imawonongeka;
- (3) Pali zomangira zozizira pamtunda;
- (4) Kusiyana kwa kutentha pakati pa nkhungu ndi chitsulo chamadzimadzi ndikokulirapo, komwe kumathandizira kuwonongeka kwa nkhungu;
- (5) Pali mitundu kapena zipsera pamwamba pa nkhungu;
- (6) Kusokonezeka
Kutentha kwambiri kwa nkhungu kumatha kuyambitsa:
- (1) Nkhungu kumamatira ndi mapindikidwe;
- (2) Kuchulukitsa kwa ogwiritsira ntchito kumasula ndikuthandizira kuwonongeka;
- (3) Kupondereza mayimbidwe kuti afalikire;
- (4) Gawo losunthika la nkhungu sachedwa kulephera komanso kufulumira;
- (5) Pali thovu kumtunda;
- (6) Pali mabowo ocheperako mkati.
Kufa makina opangira nkhungu otentha nthawi zambiri amagwiritsa ntchito mafuta ngati sing'anga, ndipo kutentha kogwira ntchito kumatha kufikira 320 ° C. Koma pali zosiyana, monga kuzirala kwa mphukira ndi makina ena a chipinda chotentha amafa akuponyera makina. Pofuna kupewa moto, madzi oponderezedwa amatha kugwiritsidwa ntchito ngati sing'anga popewa kutentha kwa mpweya pa 140 ° C. Makina ozizira osapanikizika amatha kugwiritsidwa ntchito pansi pa 95 ℃.
Mu ndondomeko kufa akuponya, kuthira kutentha, kudzazidwa nthawi, kuthira kuthamanga ndi kutentha nkhungu. Magawo Izi zokhudzana kwambiri ndi kufa kuponyera quality, linanena bungwe ndi moyo nkhungu. Mu kupanga kufa-akuponya, kufa-akuponya otentha makina nkhungu bwino ndi luso la mbali kufa-akuponya ndi ziziyenda kutentha, ndi ntchito yake ndi zotsatira zake ndi kudziwonetsera.
Chonde sungani komwe adachokera ndi adilesi iyi kuti musindikizenso: Udindo wa Die-akuponya Hot Nkhungu Machine Mu Kutentha Control Amwalira
Minghe Kampani Yoponyera ali odzipereka kupanga ndi kupereka zabwino ndi magwiridwe antchito a Kutayira Mbali (zitsulo zoponyera magawo osiyanasiyana zimaphatikizapo Woonda-Wall Die kuponyera,Kutentha Kwambiri Kuponyera,Cold Chamber Die Casting), Round Service (Ntchito Yoponyera Akafa,Cnc Machining,Kupanga Zinthu, Pamwamba pa Chithandizo) .Mtundu uliwonse wa Aluminium die kuponyera, magnesium kapena Zamak / zinc kufa kuponyera ndi zofunikira zina ndizolandilidwa kuti mutilankhule.
Motsogozedwa ndi ISO9001 ndi TS 16949, Njira zonse zimachitika kudzera pamakina opanga makina otsogola, makina a 5-axis, ndi malo ena, kuyambira ma blasters mpaka makina ochapira a Son Son.Minghe alibe zida zapamwamba komanso ali ndi akatswiri gulu la akatswiri odziwa ntchito ndi oyang'anira kuti mapangidwe kasitomala akwaniritsidwe.
Wopanga mgwirizano wopanga kufa. Mphamvu zimaphatikizapo magawo ozizira a aluminium die akuponya kuchokera ku 0.15 lbs. mpaka 6 lbs., kusintha mwachangu kukhazikitsidwa, ndi makina. Ntchito zowonjezera zimaphatikizapo kupukuta, kunjenjemera, kudodometsa, kuwombera mfuti, kupenta, zokutira, zokutira, msonkhano, ndi zida. Zipangizo zomwe zimagwiritsidwa ntchito ndizophatikiza ma alloys monga 360, 380, 383, ndi 413.
Zinc kufa kuponyera kapangidwe ka ntchito / ntchito zofananira zamakono. Makonda opanga mwatsatanetsatane wa zinc kufa. Kuponyera kwakung'ono, kuponyedwa mwamphamvu, kuponyedwa kosiyanasiyana, zopangidwa ndi nkhungu, mayendedwe amtundu ndi odziyimira payokha komanso zotsekera zotsekedwa zimatha kupangidwa. Zokongoletsa zimatha kupangidwa kutalika ndi mulifupi mpaka 24 mkati. Mu +/- 0.0005 in. Kulolerana.
ISO 9001: 2015 wopanga wa magnesium wamtundu wakufa, Mphamvu zake zimaphatikizapo kuponyera kwa magnesium kufa mpaka 200 ton chipinda chotentha & 3000 chipinda chozizira, kupanga zida, kupukuta, kuumba, kusinthanitsa, ufa & kupaka kwamadzi, QA yathunthu ndi kuthekera kwa CMM , msonkhano, kulongedza & kutumiza.
ITAF16949 yotsimikizika. Ntchito Yowonjezera Yowonjezera Phatikizani kuponyedwa kwa ndalama,kuponya mchenga,Kukongoletsa, Anataya zathovu kuponyera,Kuponyera kwamakedzana,Kuponyera Kutulutsa,Permanent Mold KuponyeraZolimba zimaphatikizaponso EDI, thandizo la uinjiniya, kutengera kolimba komanso kukonza kwina.
Akuponya Makampani Zolemba Pazigawo za: Magalimoto, Mabasiketi, Ndege, Zida zoyimbira, Watercraft, Zipangizo zamagetsi, Sensor, Models, Zipangizo zamagetsi, Zitseko, Mawotchi, Makina, Ma Injini, Mipando, Zodzikongoletsera, Ma Jigs, Telecom, Kuunikira, Zipangizo Zachipatala, Zithunzi za zithunzi, Ma Robot, Ziboliboli, Zomvera, Zida Zamasewera, Zida, Zoseweretsa ndi zina zambiri.
Kodi tingakuthandizeni kuchita chiyani?
∇ Pitani patsamba lofikira Akuponya China
→Zida zoponyera-Peza zomwe tachita.
→ Malingaliro Owonjezeka Pafupi Ntchito Zamachitidwe Akufa
By Wopanga Minghe Die Casting | Magulu: Nkhani Zothandiza |Zofunika Tags: Zotayidwa kuponyera, Kutaya Zinc, Kuponyera Magnesium, Kutumiza Titanium, Kuponya Chitsulo chosapanga dzimbiri, Kutayira Mkuwa,Kuponyera Mkuwa,Akuponya Video,Mbiri ya Kampani,Zotayidwa Die kuponyera | Ndemanga Off