Momwe Mungachotsere Zinyalala
Zimayambitsa mano
- Makulidwe a gawo lililonse la malonda ndi osiyana
- Kupanikizika kokwanira mkati mwa nkhungu
- Kuzirala kwa nkhungu kosakwanira
- Kupunduka chifukwa chosakwanira nthawi yozizira
Zomwe zimagwirizana
- Pokonza zinthu, zokometsera ndizomwe zimachitika pafupipafupi pazinthu zosafunikira. Pulasitiki yomwe idalowetsedwa mu nkhungu imatsika ikakhazikika. Gawo loyambirira kuzirala, ndiye kuti, pamwamba pamalimba, ndipo thovu limapangidwira mkati. Zomwe zimatchedwa kuti dents ndi gawo lozizira pang'onopang'ono limatulutsa mawonekedwe owoneka bwino a concave potengera kuwira kwa kuwira.
- Zipangizo zokhala ndi shrinkage yayikulu zimakhalanso ndi zibangili. Mukamasintha zinthu zoumbiramo kuti muchotse mano, mawonekedwe ake ayenera kukhazikitsidwa komwe shrinkage ndiyochepa. Ndiye kuti, kutentha kwa nkhungu ndi kutentha kwa mbiya kumachepa, ndipo kupanikizika kwa jakisoni kumawonjezeka, koma ziyenera kudziwidwa kuti izi zimatha kupangitsa kutsalira kwamkati.
- Chifukwa malowo ndi abwino kukhala osawonekera, ngati samakhudza mawonekedwe, amawakonza dala kukhala mawonekedwe owola pa nkhungu, monga mbewu, mbewu, ndi zina zambiri. kuchepetsa kutentha nkhungu kuchepetsa kumaliza. Komabe, mano akachitika munjirazi, zimakhala zovuta kukonza zopukutidwa.
The Anakonza
- Instant: Wonjezerani kupanikizika kwa jakisoni, onjezani nthawi yogwirizira jakisoni, kuchepetsa kutentha kwa mbiya ndi kutentha kwa nkhungu, ndikukakamiza kuziziritsa komwe kumapangidwa mano.
- Nthawi yayifupi: Lembani madzi osefukirawo (Chithunzi A). Pakakhala malo opapatiza m'mphepete mwa chinthu chomwe chimapangidwira, pangani gawo ili lokulirapo (Chithunzi B).
- Kutalika: Kusiyana kwa makulidwe azinthu zopangidwa kuyenera kupewedwa kwathunthu. Kulimbitsa nthiti zomwe zimakonda kupindika, mawonekedwe atali komanso opapatiza ayenera kukhala afupikitsa momwe angathere
Kusiyana kwa zida
Zipangizo zokhala ndi zikuluzikulu zazikulu zoumba zili ndi zopindika zazikulu. Mwachitsanzo, PE, PP, ngakhale nthiti zowonjezerapo pang'ono, zimatulutsa zibowo.
Zothandizira
- Kutentha kukatsika mpaka kufika poti palibe mano opangidwa, ngati zinthu zomwe zili mchimbudzi zikadapitilizidwa, ziyenera kuganiziridwa kuti sipadzakhala mano. Kupanikizika kwa nkhungu kwa zinthu zomwe zimazungulira nkhunguyo ndi kupsinjika kwa static, komwe sikofanana nthawi zonse. Kupanikizika kwa gawo lomwe lili pafupi ndi chipatacho ndi kwakukulu. Ngati nkhaniyo ili m'mbali mwake, chifukwa chakufalitsa kwa ngodya iliyonse, kusiyana pakati pa gawo lomwe lili pafupi ndi chipata ndi malo akutali kwambiri ndi chipata ndikocheperako poyerekeza ndi kukakamizidwa konse, ndipo palibe kukhumudwa komwe kudzachitike . Ndikothekanso kupeza zinthu popanda zotsalira zamkati. Gawo lina lazinthuzo zikafika kumalo ovuta, malowa amakhala ndi kuthamanga kwambiri, ndipo kukakamizidwa m'malo ena kumachepa, zomwe zimayambitsa zibowo. Gawo ili lapanopanikizika kwambiri ndi kupsinjika kwamkati mwazogulitsazo. Mu mkhalidwe wabwino, kutentha kwakuthupi kumatuluka ndi kutentha kwa nkhungu, kutentha kwa zinthu kumakhala bwino, ndipo jakisoniyo amakhala pansi pakumangika kwadzikoli.
- Mukasintha zinthu zoumba, kuphatikiza kutentha, kupanikizika, ndi nthawi ziyenera kukonzekera pasadakhale, ndipo zotsatira zake zitha kudziwika koyambirira potsatira dongosolo. Choyamba, nthawi ikakhala yayitali kwambiri, ndikosavuta kudziwa kusintha kwakung'ono kulikonse pakapanikizika. Tiyenera kudziwa kuti zotsatira zakusintha kwa kutentha kumapezeka, ndipo zotsatira zake ziyenera kukhala zotsatira zakomwe kutentha kumatsika pambuyo pa jakisoni wazinthuzo.
Chonde sungani komwe adachokera ndi adilesi iyi kuti musindikizenso: Momwe Mungachotsere Zinyalala
Minghe Kampani Yoponyera ali odzipereka kupanga ndi kupereka zabwino ndi magwiridwe antchito a Kutayira Mbali (zitsulo zoponyera magawo osiyanasiyana zimaphatikizapo Woonda-Wall Die kuponyera,Kutentha Kwambiri Kuponyera,Cold Chamber Die Casting), Round Service (Ntchito Yoponyera Akafa,Cnc Machining,Kupanga Zinthu, Pamwamba pa Chithandizo) .Mtundu uliwonse wa Aluminium die kuponyera, magnesium kapena Zamak / zinc kufa kuponyera ndi zofunikira zina ndizolandilidwa kuti mutilankhule.
Motsogozedwa ndi ISO9001 ndi TS 16949, Njira zonse zimachitika kudzera pamakina opanga makina otsogola, makina a 5-axis, ndi malo ena, kuyambira ma blasters mpaka makina ochapira a Son Son.Minghe alibe zida zapamwamba komanso ali ndi akatswiri gulu la akatswiri odziwa ntchito ndi oyang'anira kuti mapangidwe kasitomala akwaniritsidwe.
Wopanga mgwirizano wopanga kufa. Mphamvu zimaphatikizapo magawo ozizira a aluminium die akuponya kuchokera ku 0.15 lbs. mpaka 6 lbs., kusintha mwachangu kukhazikitsidwa, ndi makina. Ntchito zowonjezera zimaphatikizapo kupukuta, kunjenjemera, kudodometsa, kuwombera mfuti, kupenta, zokutira, zokutira, msonkhano, ndi zida. Zipangizo zomwe zimagwiritsidwa ntchito ndizophatikiza ma alloys monga 360, 380, 383, ndi 413.
Zinc kufa kuponyera kapangidwe ka ntchito / ntchito zofananira zamakono. Makonda opanga mwatsatanetsatane wa zinc kufa. Kuponyera kwakung'ono, kuponyedwa mwamphamvu, kuponyedwa kosiyanasiyana, zopangidwa ndi nkhungu, mayendedwe amtundu ndi odziyimira payokha komanso zotsekera zotsekedwa zimatha kupangidwa. Zokongoletsa zimatha kupangidwa kutalika ndi mulifupi mpaka 24 mkati. Mu +/- 0.0005 in. Kulolerana.
ISO 9001: 2015 wopanga wa magnesium wamtundu wakufa, Mphamvu zake zimaphatikizapo kuponyera kwa magnesium kufa mpaka 200 ton chipinda chotentha & 3000 chipinda chozizira, kupanga zida, kupukuta, kuumba, kusinthanitsa, ufa & kupaka kwamadzi, QA yathunthu ndi kuthekera kwa CMM , msonkhano, kulongedza & kutumiza.
ITAF16949 yotsimikizika. Ntchito Yowonjezera Yowonjezera Phatikizani kuponyedwa kwa ndalama,kuponya mchenga,Kukongoletsa, Anataya zathovu kuponyera,Kuponyera kwamakedzana,Kuponyera Kutulutsa,Permanent Mold KuponyeraZolimba zimaphatikizaponso EDI, thandizo la uinjiniya, kutengera kolimba komanso kukonza kwina.
Akuponya Makampani Zolemba Pazigawo za: Magalimoto, Mabasiketi, Ndege, Zida zoyimbira, Watercraft, Zipangizo zamagetsi, Sensor, Models, Zipangizo zamagetsi, Zitseko, Mawotchi, Makina, Ma Injini, Mipando, Zodzikongoletsera, Ma Jigs, Telecom, Kuunikira, Zipangizo Zachipatala, Zithunzi za zithunzi, Ma Robot, Ziboliboli, Zomvera, Zida Zamasewera, Zida, Zoseweretsa ndi zina zambiri.
Kodi tingakuthandizeni kuchita chiyani?
∇ Pitani patsamba lofikira Akuponya China
→Zida zoponyera-Peza zomwe tachita.
→ Malingaliro Owonjezeka Pafupi Ntchito Zamachitidwe Akufa
By Wopanga Minghe Die Casting | Magulu: Nkhani Zothandiza |Zofunika Tags: Zotayidwa kuponyera, Kutaya Zinc, Kuponyera Magnesium, Kutumiza Titanium, Kuponya Chitsulo chosapanga dzimbiri, Kutayira Mkuwa,Kuponyera Mkuwa,Akuponya Video,Mbiri ya Kampani,Zotayidwa Die kuponyera | Ndemanga Off